Effect of lime additions and bulk chromium content on
The reason being that lime was originally added as 10%wt of the feed stream in the processing of Merensky ore to act as a fluxing agent. With the new furnace design and higher power densities the slag are maintained at 200oC to 350oC higher than when Merensky ore was smelted.